2507 Duplex Stainless Steel Plate

8
Oct-31/2024

2507 Duplex Stainless Steel Plate Description2507(UNS S32750) is an ultra-duplex stainless steel containing 25% chromium, 4% molybdenum and 7% nickel. It is designed for demanding applications that require excellent strength and corrosion resistance, such as chemical processes, petrochemicals and se



2507 Duplex Stainless Steel Plate Description

2507(UNS S32750) is an ultra-duplex stainless steel containing 25% chromium, 4% molybdenum and 7% nickel. It is designed for demanding applications that require excellent strength and corrosion resistance, such as chemical processes, petrochemicals and seawater equipment. The steel has excellent resistance to chloride stress corrosion cracking, high thermal conductivity and low coefficient of thermal expansion. High chromium, molybdenum and nickel levels provide excellent resistance to pitting, crevice corrosion and general corrosion.


Product Parameters

Product Name

2507 Duplex Stainless Steel Plate

Type

Plate

Thickness

0.3mm-200mm

Length

2000mm, 2438mm, 3000mm, 5800mm, 6000mm, 12000mm, etc.

Width

40mm-600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc.

Standard

ASTM, AISI, JIS, GB, DIN, EN, etc.

Surface

BA, 2B, NO.1, NO.4, 4K, HL, 8K, etc.

Scope of Application

Widely used in high temperature and electrical industry, medical equipment construction, chemical, food industry, agriculture and ship parts, food and beverage packaging,

Kitchen supplies, trains, airplanes, conveyor belts, vehicles, bolts, nuts, springs and screens, etc.

Certificate

ISO, SGS, BV, etc.

Production Technology

Hot Rolling, Cold Rolling

Edge Processing

Edging, Trimming

 

Chemical Composition

C

Si

Mn

Cr

Ni

Mo

S

P

≤ 0.03

≤ 0.8

≤ 1.2

24.0~26.0

6.0~8.0

3.0~5.0

≤ 0.02

≤ 0.035

 

Mechanical Properties

Tensile Strength Kb (MPa)

Yield Strength σ0.2 (MPa)

Elongation D5 (%)

Hardness

≥795

≥550

≥15

≤ 310HB

 

Physical Performance

Density(g/cm³)

Modulus of Elasticity(Gpa)

Coefficient of Thermal Expansion(10-6/°C)

Coefficient of Thermal Conductivity(W/m*K)

Resistivity(ΜΩ. cm)

7.75

200

13.0

17.0

80

 