Hastelloy B-2 Plate DescriptionThe chemical composition of Hastelloy B2platemainly includes nickel, chromium, molybdenum and a small amount of iron, tungsten and other elements. The combination of these elements gives the material excellent corrosion resistance and high
The chemical composition of Hastelloy B2 plate mainly includes nickel, chromium, molybdenum and a small amount of iron, tungsten and other elements. The combination of these elements gives the material excellent corrosion resistance and high-temperature strength. Among them, the nickel element provides good corrosion resistance, the chromium element enhances the material's corrosion resistance in an oxidizing environment, and the molybdenum element improves the material's corrosion resistance in a reducing environment. In addition, the addition of elements such as iron and tungsten further enhance the strength and hardness of the material. Hastelloy B2 plate has good processing properties and can be used for hot processing and cold processing. Among them, hot processing includes casting, hot rolling, heat treatment and other processes, while cold processing includes cold rolling, cold drawing, stamping and other processes.
Product Parameters
Product Name | Hastelloy B-2 Plate |
Thickness | 0.3mm-200mm |
Length | 2000mm, 2438mm, 3000mm, 5800mm, 6000mm, 12000mm, etc. |
Width | 40mm-600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc. |
Standard | ASTM, AISI, JIS, GB, DIN, EN, etc. |
Surface | BA, 2B, NO.1, NO.4, 4K, HL, 8K, etc. |
Certificate | ISO, SGS, BV |
Production Technology | Hot Rolling, Cold Rolling |
Chemical Composition
C | Si | P | S | Cr | Mn | Fe | Co | Ni | Mo |
0.02 max | 0.1 max | 0.04 max | 0.03 max | 1.0 max | 1.0 max | 2.0 max | 1.0 max | Remainder | 26.0 - 30.0 |
Mechanical Properties
Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
110 | 51 | 40 |
Physical Performance
Units | Temperature in°C | |
Density | 9.22 g/cm³ | 22°C |
Specific Heat | 0.089 Kcal/kg.C | Room |
Melting Range | 1370-1418°C | - |
Modulus of Elasticity | 217 KN/mm² | Room |
Electrical Resistivity | 137 µΩ.cm | 0 ° |
Coefficient of Expansion | 10.3 µm/m °C | 20-93° |
Thermal Conductivity | 11.1 w/m-° K | 0° |
Scope of Application
B- 2 is used in chemical processes, vacuum furnaces, mechanical parts in reduced pressure environments, etc.
-