Incoloy 800 Pipe

3
Nov-04/2024

Incoloy 800 Pipe DescriptionThe chemical composition of Incoloy 800 alloy consists primarilyof nickel, chromium and iron. Nickel is the main element that leads tothe corrosion resistance of the alloy, chromium enhancesthe oxidation resistance and high-temperature strength of



Incoloy 800 Pipe Description

The chemical composition of Incoloy 800 alloy consists primarily of nickel, chromium and iron. Nickel is the main element that leads to the corrosion resistance of the alloy, chromium enhances the  oxidation resistance and high-temperature strength of the alloy, and  iron provides the matrix structure of the alloy. In addition, the alloy  also contains certain amounts of elements such as carbon, silicon and  manganese to further enhance its overall performance. Incoloy 800  pipe has remarkable corrosion resistance, especially in reducing and  oxidizing media. It also has good resistance to chemicals such as  sulfuric acid, hydrochloric acid and alkaline solutions in high  temperature environments. Incoloy 800 pipes have good oxidation resistance in high temperature environments and can work at temperatures up to 1100°C for a long time. Lastly, Incoloy 800  pipes have high yield strength and creep strength and can uphold its  mechanical properties in high and low temperature environments.

 

Product Parameters

Product Name

Incoloy 800 Pipe

Outer Diameter

Round Pipe

4mm-200mm

Square Pipe

10*10mm-100*100mm

Rectangular Pipe

10*20mm-50*100mm

Wall Thickness

0.6mm-6.0mm

Length

1-6 meters, Length can be customized

Standard

ASTM, AISI, JIS, GB, DIN, EN, etc.

Surface

Black, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc.

Certificate

ISO, SGS, BV

Production Technology

Hot Rolling, Cold Rolling

 

Chemical Composition

C

Al

Si

S

Ti

Cr

Mn

Fe

Ni

Cu

0.1 max

0.15 - 0.60

1.0 max

0.015 max

0.15 - 0.60

19.0 - 23.0

1.5 max

39.5 min

30.0 - 35.0

0.75 max

 

Mechanical Properties

Tensile Strength (ksi)

0.2% Yield Strength (ksi)

Elongation% in 2 inches

75

30

30

 

Physical Performance


Units

Temperature in°C

Density

7.94 g/cm³

Room

Specific Heat

0.11 Kcal/kg.C

21°

Melting Range

1357-1385°C

-

Modulus of Elasticity

196.5 KN/mm²

20°

Electrical Resistivity

98.9 µΩ.cm

20°

Coefficient of Expansion

14.4 µm/m °C

20 - 100°

Thermal Conductivity

11.5 w/m-° K

20°

 