Hastelloy C-22 Pipe

4
Nov-04/2024

Hastelloy C-22 Pipe DescriptionThe main elements of Hastelloy C22pipeinclude cobalt, chromium, tungsten, molybdenum and small amounts of aluminum, titanium and nitrogen. Cobalt element improvesthe strength and hardness of the alloy, chromium element has an important imp



Hastelloy C-22 Pipe Description

The main elements of Hastelloy C22 pipe include cobalt, chromium, tungsten, molybdenum and small amounts of aluminum, titanium and nitrogen. Cobalt element improves the  strength and hardness of the alloy, chromium element has an important  impact on the corrosion resistance of the alloy, tungsten and molybdenum  can increase the high-temperature strength of the alloy. Moreover,  the addition of aluminum and titanium elements can refine the grains  and improve the toughness of the alloy, while the addition of nitrogen  can improve the strength and corrosion resistance of the alloy. Besides,  it has good plasticity and toughness and can work with both cold and  hot processing. Hastelloy C22 pipe also features excellent oxidation  resistance and creep resistance at high temperatures. Hastelloy C22  pipes are commonly used in aerospace, chemical industry, petroleum and  other fields because of its excellent corrosion resistance and high  temperature strength.

 

Product Parameters

Product Name

Hastelloy C-22 Pipe

Outer Diameter

Round Pipe

4mm-200mm

Square Pipe

10*10mm-100*100mm

Rectangular Pipe

10*20mm-50*100mm

Wall Thickness

0.6mm-6.0mm

Length

1-6 meters, Length can be customized

Standard

ASTM, AISI, JIS, GB, DIN, EN, etc.

Surface

Black, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc.

Certificate

ISO, SGS, BV

Production Technology

Hot Rolling, Cold Rolling

 

Chemical Composition

C

Si

P

S

V

Cr

Mn

Fe

Co

Ni

Mo

W

0.015 max

0.08 max

0.02 max

0.02 max

0.35 max

20.0 - 22.5

0.50 max

2.0-6.0

2.5 max

Remainder

12.5 - 14.5

2.5 - 3.5

 

Mechanical Properties

Tensile Strength (ksi)

0.2% Yield Strength (ksi)

Elongation% in 2 inches

100

45

45

 

Physical Performance


Units

Temperature in°C

Density

8.69 g/cm³

24°C

Specific Heat

0.093 Kcal/kg.C

52°

Melting Range

1357-1399°C

-

Modulus of Elasticity

205.5 KN/mm²

-

Electrical Resistivity

113.7 µΩ.cm

24 °

Coefficient of Expansion

12.4 µm/m °C

24-93°

Thermal Conductivity

10.1 w/m-° K

48°

 

Scope of Application

C-  276 alloy is used in pesticide production, phosphoric acid production,  pickling system, plate heat exchanger, selective leaching system, SO2  cooling tower, sulfonation system, shell and tube heat exchanger,  surfacing welding valve, etc.


-