Incoloy 800 Coil DescriptionThe chemical composition of Incoloy 800 alloy consists mainly of nickel, chromium and iron. Among them, nickel is the main element that improves the corrosion resistance of the alloy, chromium helps enhance the oxidation resistance and high-tempera
The chemical composition of Incoloy 800 alloy consists mainly of nickel, chromium and iron. Among them, nickel is the main element that improves the corrosion resistance of the alloy, chromium helps enhance the oxidation resistance and high-temperature strength of the alloy, and iron provides the matrix structure of the alloy. In addition, the alloy also contains certain amounts of elements such as carbon, silicon and manganese to further enhance its overall performance. Incoloy 800 coil has very good corrosion resistance, especially in reducing and oxidizing media. It also has good resistance to chemicals such as sulfuric acid, hydrochloric acid and alkaline solutions in high temperature environments. Incoloy 800 coil has good oxidation resistance in high temperature environments and can work at temperatures up to 1100°C for a long time. Lastly, Incoloy 800 coil has high yield strength and creep strength and can maintain its mechanical properties in high and low temperature environments.
Product Parameters
Product Name | Incoloy 800 Coil |
Thickness | 2.5mm-10.0 mm |
Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc. |
Width | 610-2000 mm |
Standard | ASTM, AISI, JIS, GB, DIN, EN, etc. |
Surface | BA, 2B, NO.1, NO.4, 4K, HL, 8K, etc. |
Certificate | ISO, SGS, BV |
Production Technology | Hot Rolling, Cold Rolling |
Chemical Composition
C | Al | Si | S | Ti | Cr | Mn | Fe | Ni | Cu |
0.1 max | 0.15 - 0.60 | 1.0 max | 0.015 max | 0.15 - 0.60 | 19.0 - 23.0 | 1.5 max | 39.5 min | 30.0 - 35.0 | 0.75 max |
Mechanical Properties
Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
75 | 30 | 30 |
Physical Performance
Units | Temperature in°C | |
Density | 7.94 g/cm³ | Room |
Specific Heat | 0.11 Kcal/kg.C | 21° |
Melting Range | 1357-1385°C | - |
Modulus of Elasticity | 196.5 KN/mm² | 20° |
Electrical Resistivity | 98.9 µΩ.cm | 20° |
Coefficient of Expansion | 14.4 µm/m °C | 20 - 100° |
Thermal Conductivity | 11.5 w/m-° K | 20° |
Scope of Application
The most common applications are heat treatment equipment, petrochemical pyrolysis piping systems, electric heating unit jackets and food processing equipment.
-