Incoloy 925 Bar

4
Nov-04/2024

Incoloy 925 Bar DescriptionIncoloy 925 alloy is primarilycomposed of nickel, chromium, iron and other elements, and also contains a certain amount of aluminum, titanium. This alloy has good corrosion resistance and can maintain stable performance in oxidizing and reducing &nb



Incoloy 925 Bar Description

Incoloy 925 alloy is primarily composed  of nickel, chromium, iron and other elements, and also contains a  certain amount of aluminum, titanium. This alloy has good corrosion  resistance and can maintain stable performance in oxidizing and reducing  environments. In addition, Incoloy 925 also has good high-temperature  strength and creep properties, and can maintain good mechanical  properties in high-temperature environments. Other excellent properties  include excellent welding and manufacturing processability. Besides,  Incoloy 925 bars can resist oxidation and hot corrosion in  high-temperature oxidizing environments. One thing to note is Incoloy  925 bar shows good resistance to stress corrosion cracking in  chlorine-containing media and is suitable for seawater environments and  chemical process applications containing chlorides.

 

Product Parameters

Product Name

Incoloy 925 Bar

Outer Diameter

Round Bar

4mm-500mm

Hexagon Bar

18mm-57mm (11/16″ to 2-3/4″)

Square Bar

18mm-47mm (11/16″ to 1-3/4″)

Flat Steel

1/2 "to 10", Thickness: 2mm-150mm, Can provide customized

Length

1-6 meters, Length can be customized

Standard

ASTM, AISI, JIS, GB, DIN, EN, etc.

Surface

Black, Bright Polished, Rough Turning, Matt Surface Treatment, NO.4, BA, etc.

Certificate

ISO, SGS, BV

Production Technology

Hot Rolling, Cold Rolling

 

Chemical Composition

C

Al

Si

P

S

Ti

Cr

Mn

Fe

Ni

Cu

Nb

Mo

0.03 max

0.1 - 0.5

0.5 max

0.03 max

0.03 max

1.9 - 2.4

19.5 - 22.5

1.0 max

22.0 min

42.00-46.00

1.5 - 3.0

0.5 max

2.5 - 3.5

 

Mechanical Properties

Tensile Strength (ksi)

0.2% Yield Strength (ksi)

Elongation% in 2 inches

85

35

30

 

Physical Performance


Units

Temperature in°C

Density

8.14 g/cm³

Room

Specific Heat

0.105 Kcal/kg.C

Room

Melting Range

1370-1400°C

-

Modulus of Elasticity

196 KN/mm²

20°

Electrical Resistivity

113 µΩ.cm

25°

Coefficient of Expansion

14.1 µm/m °C

25 - 100°

Thermal Conductivity

11.1 w/m-° K

25°

 

Scope of Application

This  superalloy is used in a variety of industries, such as aerospace,  chemical processing, marine engineering, pollution control equipment and  nuclear reactors.


-