Incoloy 800 Bar

3
Nov-04/2024

Incoloy 800 Bar DescriptionThe chemical composition of Incoloy 800 alloy consists mainly of nickel, chromium and iron. Nickel is the main element thatleads toimprovedcorrosion resistance of the alloy, chromium helps enhance the oxidation resistance and high-temperature



Incoloy 800 Bar Description

The chemical composition of Incoloy 800 alloy consists mainly of nickel, chromium and iron. Nickel is the main element that leads to improved corrosion  resistance of the alloy, chromium helps enhance the oxidation  resistance and high-temperature strength of the alloy, and iron forms the matrix structure of the alloy. In addition, the alloy also integrates certain amounts of elements such as carbon, silicon and manganese to further enhance its overall performance. Incoloy 800  bar is highly resistant to corrosion from reducing and oxidizing media.  It also has good resistance to chemicals such as sulfuric acid,  hydrochloric acid and alkaline solutions in high temperature  environments. Incoloy 800 bar comes with good oxidation resistance in high temperature environments and can work at temperatures up to 1100°C for a long time. Lastly, Incoloy 800  bar can maintain its mechanical properties in high and low temperature  environments, with high yield strength and creep strength.

 

Product Parameters

Product Name

Incoloy 800 Bar

Outer Diameter

Round Bar

4mm-500mm

Hexagon Bar

18mm-57mm (11/16″ to 2-3/4″)

Square Bar

18mm-47mm (11/16″ to 1-3/4″)

Flat Steel

1/2 "to 10", Thickness: 2mm-150mm, Can provide customized

Length

1-6 meters, Length can be customized

Standard

ASTM, AISI, JIS, GB, DIN, EN, etc.

Surface

Black, Bright Polished, Rough Turning, Matt Surface Treatment, NO.4, BA, etc.

Certificate

ISO, SGS, BV

Production Technology

Hot Rolling, Cold Rolling

 

Chemical Composition

C

Al

Si

S

Ti

Cr

Mn

Fe

Ni

Cu

0.1 max

0.15 - 0.60

1.0 max

0.015 max

0.15 - 0.60

19.0 - 23.0

1.5 max

39.5 min

30.0 - 35.0

0.75 max

 

Mechanical Properties

Tensile Strength (ksi)

0.2% Yield Strength (ksi)

Elongation% in 2 inches

75

30

30

 

Physical Performance


Units

Temperature in°C

Density

7.94 g/cm³

Room

Specific Heat

0.11 Kcal/kg.C

21°

Melting Range

1357-1385°C

-

Modulus of Elasticity

196.5 KN/mm²

20°

Electrical Resistivity

98.9 µΩ.cm

20°

Coefficient of Expansion

14.4 µm/m °C

20 - 100°

Thermal Conductivity

11.5 w/m-° K

20°

 

Scope of Application

The  most common applications are heat treatment equipment, petrochemical  pyrolysis piping systems, electric heating unit jackets and food  processing equipment.


-